F-type timber with fire retardant and corrosion and dimensionally stable multifunctional type wood protectants. Retardant wood has a strong anti-corrosion, dimensional stability, strong anti-moth efficacy of the product arsenic, chromium, copper, and persistent organic pollutants, lower processing costs, preparation of a good solution can be recycled, in line with the State Environmental Protection requirements, compliance with EU RoHS directive restricts the use of PBB and PBDE testing requirements under the treated wood does not change the original color. Rapid response activity was converted to the ammonium nitrogen compound flame retardant by a combination of tannins and phenolic compounds, and wood. Further long-term effective change combustion properties of wood.
First, the technical parameters black pvc lattice panels:
1, Appearance: transparent liquid
2, stability: stability factor strong
3 Solubility: soluble in water.
4 Ion: Nonionic
5, permeability: 30 seconds (poplar veneer pre-treatment)
6, the effective active content: 80%
7, the viscosity (25 ℃): 12 ~ 15 mpa.s
Second, the scope:
Wooden treasure-F-type flame retardant mainly used in wood huts, wooden house, wooden resorts, wooden landscape, wooden structures, grass roofs, wooden hall, hotel decoration wood products, a variety of plate (plywood) joinery semi-finished and finished products, wood flooring, wood furniture semi-finished products, finished products, wooden crafts, moldings, wood siding and other fire-retardant protective treatment.
Third, the product features inexpensive outdoor flooring :
Wooden treasure-F-type flame retardant timber with a wide range of protection, instant super penetration, anti-loss performance, generate instant injection of nitrogen ammonium compounds insoluble after curing the wood, not volatile, rain or soil moisture and less susceptible to influence drain, weathering resistance, does not affect the paint application, without reducing the strength of wood and insulation resistance, dimensional stability and improved wood preservative characteristics.
The use of methods: First, clean up the attachments before operating a clean wood surface, and then select and water mixture is diluted proportionately.
Configured as an aqueous solution, subjected to vacuum pressure, dipping treatment and spraying paint
A vacuum pressure method: It is recommended to use a concentration of 10% -15%, with vacuum pressure treatment to fully penetrate the calculation agent, the general drug loading 20 ~ 30kg/m3 to meet national building materials and wood products of combustion performance (GB8624-2006) requirements B2, B1 level
2, the immersion method: It is recommended to use a concentration of 15-20% with water to completely cover the wood for the standard 15-30 minutes soaking time brown vinyl fence panels
3, brushing spray: It is recommended to use a concentration of 20% -25% of the wood surface to fully absorb that (complete wetting of the standard) paint spray area 20-25 square / KG, recommendations and brushing 2 times for spraying, Brushing twice a spray interval of 2-4 hours
V. Notes:
1, must be cleaned of dust and dirt and clean wood surface operation, to avoid affecting the liquid permeability and reusability
2, when the job accidentally come into contact with the skin, rinse with water should be promptly
3, treated wood should not be used for food packaging
4, the operating and storage should be away from children. Agents used and waste should not be discarded.